[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: HDPE SRSG DISK?
Hi
Is it possible to glue Lexan and the material of the print circuit (G-10 ?)
together ? If it's possible you could sandwich it like 1/16" G-10 ,1/8" lexan ,
1/16" g-10, 1/8 lexan , 1/16 G-10. More easy to machine than solid G-10
and more
resistant to heat than lexan .
Luc Benard
Tesla list wrote:
> Original poster: Terry Fritz <twftesla-at-uswest-dot-net>
>
> Hi Mike,
>
> The stuff is too soft and melts at such a low temperature that the
> thing
> would just be a mess. I made two gaps from HDPE. One melted and the
other is
> just too unstable especially under the spinning stresses. Lexan and, of
> course, the phenolics are a far better choice.
>
> Cheers,
>
> Terry