[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [TCML] Varnishing Secondary
The gallon of Dolphs I got from DC,did quite well on my large secondary
16" by 80" wound w/17g magnet wire,fiberglass secondary.
The gallon covered it about twice,,,no slippage,
Joe in Texas
On Wed, 08 Apr 2009 17:30 -0700, "DC Cox" <resonance@xxxxxxxxxxxx>
wrote:
> I use 2 prior to winding. Especially heavy coats on inside.
>
> Then, 5 thin coats after winding. Sand very lightly between first 4
> coats
> with 1000 grit to remove bubbles, wipe down with an alcohol soaked tack
> rag
> (no lint), and then do not sand the
> last coat. I use Dolph's AC-43 --- made especially for this purpose.
>
> Dr. Resonance
>
>
>
>
> On Wed, Apr 8, 2009 at 2:59 PM, Matthew Stevens
> <truesoutherngeek@xxxxxxxxx>wrote:
>
> > I was wondering how many coats of varnish would be advisable for the
> > outside
> > of the secondary coil? I put two coats on mine, but have read conflicting
> > things about how many is best. Does anyone have any opinions?
> >
> > Thanks,
> > Matthew
> > _______________________________________________
> > Tesla mailing list
> > Tesla@xxxxxxxxxxxxxx
> > http://www.pupman.com/mailman/listinfo/tesla
> >
> _______________________________________________
> Tesla mailing list
> Tesla@xxxxxxxxxxxxxx
> http://www.pupman.com/mailman/listinfo/tesla
--
johnbrooks@xxxxxxxxxxx
--
http://www.fastmail.fm - One of many happy users:
http://www.fastmail.fm/docs/quotes.html
_______________________________________________
Tesla mailing list
Tesla@xxxxxxxxxxxxxx
http://www.pupman.com/mailman/listinfo/tesla