Temperature is very important for the solvent to work well. The warmer it
is the faster it will work. I have found the same thing my self depotting a
few NST's. Also, agitation can make the process go much faster. If you can
come with a way to agitate the solvent it will dissolve the tar much faster.
A motor with an offset weight will vibrate the bath. But becarful and
sheild any electric pumps or motors from the solvent and fumes or your
transfomer will be charcoal! :-)
I was thinking of using a fuel pump to circulate the gasoline in a 5 gal
pail. I think the "Flowing" effect of the solvent will reduce the time to
depot drastically, although I haven't had time to try it yet.
Bob.
>From: Tesla List <tesla-at-pupman-dot-com>
>To: tesla-at-pupman-dot-com
>Subject: Mutant Tar!!
>Date: Mon, 24 Apr 2000 20:47:17 -0600
>
>Original Poster: "Brad DiGiovine" <Guido28-at-mediaone-dot-net>
>
>to all,
>
>i have had a NST sitting in gasoline for the past month unpotting and it
>is still not all off. I can barely see the windings. Has anyone else
>ever run into this? my 12kv30ma NST only took a week, and this 15kv30ma
>is taking a lot longer. Are there better solvents for unpotting than
>gasoline? thanks
>