[Prev][Next][Index][Thread]
Re: oil filled resonators
Bert,
Thanks for this valuable information. But this is rather
distressing. It looks as if some of the "best" plastics for our work
are in fact the worst when it comes to oil immersion.
> 25 Deg
> Typical With
> Common Trade Mineral
> Symbol: Name Oil
> ======= ========= =======
> ABS Cycolac *
> CAB Butyrate *
> CPVC - A
> Epoxy Glass G10 A
> Epoxy - A
> HDPE - B
> LDPE - B
> POM Delrin A
> PA 6 Nylon 6 A
> PA 66 Nylon 66 A
> PC Lexan C
> PET Mylar A
> PI Kapton A
> PMMA Plexiglas B
> PP - C
> PS - D
> PTFE Teflon A
> PUR - *
> PVC - A
> PVF - A
> PVDF Kynar A
>
> A: No significant impact
> B: Slight Swelling and absorbtion
> C: Moderate Attack. Limited Life
> D: Decomposes/Dissolves
> *: No Data Available
Polypropylene scores a "C" and Lexan!! :(
Polyethylene scores "B" as does PMMA :(
Enjoy? I think not but definitely worth knowing!
Thanks,
Malcolm