> Secondary: two polyethylene trash cans glued together 7.5" to
> 8" to 7.5" 20 5/8" long.
> wound with 22 A.W.G. magnet wire. 2 coats of water
> based polyurethane over it. Oops!
Is water based polyurethane a bad coating to use? I was just thinking of
using it!
Kevin M. Conkey
[Yes, it's bad (for coiling). Don't use it. I have and got terrible results.